Vinylester resin thixotropic, pre-accerelated suitable for hand lamination. This resin has a high chemical resistence towards a wide range of substances.


Dosing of initiator: 100g resin + 1,25 ml NOROX 925H/Promox P250TX.
  • Chemical and physical characteristics of liquid resin
    Appearance Cloudy liquid
    Viscosity @25°C (Brookfield RVF Spindle#3@60rpm) 450 - 550 mPa.s
    Thixotropic index 3,0 - 3,8
    Curing conditions: 100 g resin + 1,25 g MEKP50
    Gel time @25°C 27 - 35 minutes
    Exothermal peak 155 - 175 °C
    Gel to peak time 10 - 15 minutes
    Styrene content 29 - 33 %
    Water content Max 0,1 %
  • Resin classification
    vinilészter
    Weight
    1.2 kg/db